Abstrakt: This paper focuses on the difficulty with Vickers hardness evaluation of SiOC materials. To evaluate it, diagonals of an indent are crucial. Due to stress relaxation in experimental material it was not possible to evaluate it in the whole range of experimental temperatures. As experimental materials were used two types of commercialy available polysiloxane resins, pyrolysed in range from 400 to 1000°C.
Klíčová slova: 3D reconstruction; ceramics; glass; indent; polysiloxane; resin; SiOC; Vickers hardness
Číslo projektu: GAP107/12/2445 (CEP), EE2.3.20.0214
Poskytovatel projektu: GA ČR, GA MŠk
Zdrojový dokument: Multi-level Design of Advanced Materials, ISBN 978-80-214-5146-9

Instituce: Ústav fyziky materiálů AV ČR (web)
Informace o dostupnosti dokumentu: Dokument je dostupný v příslušném ústavu Akademie věd ČR.
Původní záznam: http://hdl.handle.net/11104/0258103

Trvalý odkaz NUŠL: http://www.nusl.cz/ntk/nusl-203192


Záznam je zařazen do těchto sbírek:
Věda a výzkum > AV ČR > Ústav fyziky materiálů
Konferenční materiály > Příspěvky z konference
 Záznam vytvořen dne 2016-03-08, naposledy upraven 2021-11-24.


Není přiložen dokument
  • Exportovat ve formátu DC, NUŠL, RIS
  • Sdílet