Original title:
Stress relaxation in partially pyrolysed SiOC materials
Authors:
Halasová, Martina ; Chlup, Zdeněk ; Černý, Martin ; Strachota, Adam ; Dlouhý, Ivo Document type: Papers Conference/Event: Multi-level Design of Advanced Materials, Velké Bílovice (CZ), 2015-05-28 / 2015-05-29
Year:
2015
Language:
eng Abstract:
This paper focuses on the difficulty with Vickers hardness evaluation of SiOC materials. To evaluate it, diagonals of an indent are crucial. Due to stress relaxation in experimental material it was not possible to evaluate it in the whole range of experimental temperatures. As experimental materials were used two types of commercialy available polysiloxane resins, pyrolysed in range from 400 to 1000°C.
Keywords:
3D reconstruction; ceramics; glass; indent; polysiloxane; resin; SiOC; Vickers hardness Project no.: GAP107/12/2445 (CEP), EE2.3.20.0214 Funding provider: GA ČR, GA MŠk Host item entry: Multi-level Design of Advanced Materials, ISBN 978-80-214-5146-9
Institution: Institute of Physics of Materials AS ČR
(web)
Document availability information: Fulltext is available at the institute of the Academy of Sciences. Original record: http://hdl.handle.net/11104/0258103