Morphogenesis and Viscoelastic Properties of Dimethacrylate Networks
Bystřický, Zdeněk ; Lehocký, Marián (oponent) ; Bradna, Pavel (oponent) ; Jančář, Josef (vedoucí práce)
The thesis deals with the investigation of dimethacrylate networks morphogenesis. Simple model resin mixtures used in this work were based on the monomers, which are typically employed as the components of matrix systems of dental resin composites. Kinetics and mechanisms of polymer networks formation were studied with respect to a structure of monomers, molar ratio of comonomers, and a concentration of the radical polymerization initiation system. Calculated profiles of functional groups conversion and polymerization rate were used as a basis for understanding and interpretation of mechanisms of networks morphogenesis and comparison with known models. Furthermore, kinetics of thermal degradation process was studied because it is closely related to the morphology of the networks. Then, temperature dependence of viscoelastic modulus was determined and the relationship between supramolecular structure of dimethacrylate networks and their viscoelastic response within the given temperature range was quantified. Polymerization kinetics was studied by differential photo-calorimetry (DPC) and infrared spectroscopy (FTIR). Process of thermal degradation was analyzed using thermo-gravimetric analysis (TGA). Viscoelastic parameters were measured using dynamic-mechanical analysis (DMA). Reactivity of dimethacrylate systems is derived from the molecular structure of monomers, because it affects mobility of reacting species during polymerization. Kinetics of polymerization is controlled by diffusion. Rate of diffusion is given by the monomer rigidity, concentration of functional groups, and an impact of physical interactions. The mobility restrictions, affecting growing chains, pendant side chains and free monomers, lead to monomolecular termination of macroradicals and limited degree of conversion. Since the mobility is restricted severely from the early phases of the reaction, i.e. from the gel point, phase separation is suppressed despite any potential thermodynamic instability, and the copolymerization process is random. This was confirmed by identification of single glass transition temperature in DMA experiments of copolymers. Heterogeneous character of morphogenesis is related to a varying reactivity of pendant functional groups. In the early phases of the polymerization, propagation proceeds via intramolecular attack of the radical site to the pendant, leading to the primary cycle formation. Probability of the cyclization is increased by flexibility of the monomer backbone. Heterogeneity of the curing reaction is characterized by formation of internally crosslinked structures, i.e. microgels, followed by their interconnections. On contrary, rigidity of the monomer leads to a higher effectivity of crosslinking and more homogeneous morphology of the corresponding networks. Presence of the inhomogeneities, characterized by coexistence of structurally distinct regions, is related to a two-step mechanism of thermal decomposition. Progress of the storage modulus and the glass transition temperature correlate with the network stiffness, effectivity of crosslinking, and the presence of physical interactions that reinforce the structure beyond the scope of covalent crosslinking. Structural heterogeneity is manifested by broad transition region indicating wide variations in relaxation times. Experimental data are in qualitative correlation with the numerical models that simulates kinetics of free radical network polymerization.
Uvolňování bisfenolu A a jeho analogů z dentálních rekonstrukčních materiálů
Tichý, Antonín ; Bradna, Pavel (vedoucí práce) ; Izakovičová Hollá, Lydie (oponent) ; Suchánek, Jakub (oponent)
Bisfenol A (BPA) je endokrinní disruptor, který se může uvolňovat z dentálních polymerních materiálů. Cílem této práce bylo prostudovat kinetiku dlouhodobého uvolňování BPA a jeho analogů z výplňových materiálů (kompozitů, hybridních skloionomerních cementů) a polykarbonátů používaných v zubním lékařství. Extrakty výplňových materiálů v methanolu a umělé slině byly odebrány po 1-260 dnech, u polykarbonátů po 1-84 dnech. Analýza extraktů byla provedena ultra vysoce účinnou kapalinovou chromatografií s tandemovou hmotnostní detekcí. BPA byl detekován v extraktech všech testovaných materiálů, zatímco přítomnost jeho analogů nebyla potvrzena. Nejvíce BPA se ze všech materiálů uvolnilo během prvního dne, poté uvolňování významně kleslo a u "BPA-free" kompozitů se zcela zastavilo. Uvolňování BPA z výplňových materiálů bylo nejvyšší u kompozitů s monomery na bázi BPA, následovány byly hybridními skloionomerními cementy a nejméně BPA se uvolnilo z "BPA-free" kompozitů. Zkrácená doba ozáření neměla významný vliv na celkové množství BPA uvolněného z výplňových materiálů, ale významně zvýšila jeho uvolňování během prvního dne. Z polykarbonátů bylo uvolňování BPA o několik řádů vyšší než z výplňových materiálů. Dle současného tolerovatelného denního příjmu (4 µg BPA/kg tělesné hmotnosti/den) lze použití...
Personal exposure measurement during dental nanocomposite grinding
Ždímal, Vladimír ; Ondráčková, Lucie ; Ondráček, Jakub ; Schwarz, Jaroslav ; Bradna, P. ; Roubíčková, A. ; Pelclová, D. ; Rössnerová, Andrea
The purpose of this study was to measure the personal exposure of each participant of the study and to compare the results with those of static monitoring. Personal nanoparticle sam-plers (PENS), which can simultaneously detect both nanoparticles (PM0.1) and respirable parti-cles (PMA), were used to determine personal exposure (Tsai et al., 2012). Area monitoring in-cluded measurement of mass concentrations using the Berner Low Pressure Impactor (BLPI 25/0.018 /2, Hauke GmbH, Gmunden, Austria) and the Low Volume Sampler (LV5, Sven Leckel Ingenieurbüro GmbH, Germany). The number concentrations and their size distributions were measured with the Scanning Mobility Particle Sizer (5MP5 3936, T5I Inc., USA) and the Aerody-namic Particle Sizer (APS 3321, TSI Inc., USA). Measurements with all of the above- mentioned instruments were performed in four shifts with six participants per shift. Each participant milled for 10 minutes and then remained in the room until the group finished the session, so the total exposure lasted about 70 minutes. Due to the high content of filler nanoparticles, the nanocom-posite Filtek Ultimate (body A2, 3M ESPE, USA) was selected for these measurements.
Plný tet: Stáhnout plný textPDF
Anxiozita dětí jako jeden z minoritních vlivů na prevalenci zubního kazu
Vašáková, Jana ; Bradna, Pavel (vedoucí práce) ; Merglová, Vlasta (oponent) ; Nováková, Květoslava (oponent)
Zubní kaz je preventabilní multifaktoriální infekční onemocnění, které vzniká jako výsledek spolupůsobení biologických, behaviorálních a psychosociálních faktorů. V jeho etiologii hraje roli i prostředí, ve kterém jedinec žije. Nezpochybnitelnou součástí prevence zubního kazu je složení a forma přijímané stravy, pravidelně prováděná orální hygiena, příjem fluoridů a průběžná zubní péče. Akcentovaným aspektem odborných studií je v současné době koncept "quality of life" neboli "well-being", tj. kvalita života jedince. A právě jedním z faktorů, který je v oblasti dětské stomatologie diskutován v souvislosti s kvalitou života dítěte, je "dental fear" - strach ze zubního ošetření. Příspěvkem této disertační práce k řešení výše uvedeného problému jsou čtyři předkládané na sebe navazující studie. První studie mapuje vztah zubních lékařů k dětským pacientům a hledá příčiny, proč jsou děti často odesílány na ošetření na fakultní pracoviště a ke specialistům. Druhá studie se věnuje environmentálním faktorům, které ovlivňují vnímání zubního prostředí předškolními dětmi a strachu těchto dětí z nejčastějších způsobů zubního ošetření. Třetí studie provádí hodnocení hladiny strachu ze zubního ošetření u vzorku předškolních dětí v České republice v korelaci se stavem jejich chrupu, který je vztažen ke geografické...
Opravy kompozitních rekonstrukcí v prevenci ztrát zubních tkání. Dlouhodobá odolnost vazby kompozit-kompozit v různých prostředích.
Comba, Lukáš ; Bradna, Pavel (vedoucí práce) ; Veverka, Jan (oponent) ; Roubalíková, Lenka (oponent)
v češtině Úvod: Na kompozitní rekonstrukce působí v prostředí dutiny ústní vnější prostředí a mechanická zatížení, která ovlivňují jejich fyzikální a mechanické vlastnosti. To může vést k jejich zvýšenému opotřebení, ztrátě estetických vlastností a zvýšenému riziku fraktury výplně nebo selhání jejího okrajového uzávěru s negativním dopadem na životnost rekonstrukce. Kompletní odstranění a předělání poškozené rekonstrukce je časově náročné a je obvykle spojeno s další ztrátou tvrdých zubních tkání. Možnost oprav kompozitních rekonstrukcí, jakožto minimálně invazivní alternativy k jejich kompletnímu předělání, má tudíž výrazný preventivní význam v omezení ztráty tvrdých zubních tkání a zvyšuje životnost kompozitních rekonstrukcí. Na adhezní spoj mezi opravovanou kompozitní rekonstrukcí a novým kompozitem působí v ústní dutině mechanické síly a různé chemické látky, např. tenzidy používané v zubních pastách, které mohou iniciovat jeho degradaci. Snížením povrchového napětí mohou urychlovat průnik vody do adhezního spoje a tím urychlovat hydrolýzu monomerů adheziva a snižovat pevnost vazby mezi opravovaným a novým kompozitním materiálem. Dosavadní práce ukazují, že hlavním a dosud nevyřešeným problémem oprav kompozitních rekonstrukcí je vytvoření spolehlivé a dlouhodobě odolné vazby mezi původním a...
Morphogenesis and Viscoelastic Properties of Dimethacrylate Networks
Bystřický, Zdeněk ; Lehocký, Marián (oponent) ; Bradna, Pavel (oponent) ; Jančář, Josef (vedoucí práce)
The thesis deals with the investigation of dimethacrylate networks morphogenesis. Simple model resin mixtures used in this work were based on the monomers, which are typically employed as the components of matrix systems of dental resin composites. Kinetics and mechanisms of polymer networks formation were studied with respect to a structure of monomers, molar ratio of comonomers, and a concentration of the radical polymerization initiation system. Calculated profiles of functional groups conversion and polymerization rate were used as a basis for understanding and interpretation of mechanisms of networks morphogenesis and comparison with known models. Furthermore, kinetics of thermal degradation process was studied because it is closely related to the morphology of the networks. Then, temperature dependence of viscoelastic modulus was determined and the relationship between supramolecular structure of dimethacrylate networks and their viscoelastic response within the given temperature range was quantified. Polymerization kinetics was studied by differential photo-calorimetry (DPC) and infrared spectroscopy (FTIR). Process of thermal degradation was analyzed using thermo-gravimetric analysis (TGA). Viscoelastic parameters were measured using dynamic-mechanical analysis (DMA). Reactivity of dimethacrylate systems is derived from the molecular structure of monomers, because it affects mobility of reacting species during polymerization. Kinetics of polymerization is controlled by diffusion. Rate of diffusion is given by the monomer rigidity, concentration of functional groups, and an impact of physical interactions. The mobility restrictions, affecting growing chains, pendant side chains and free monomers, lead to monomolecular termination of macroradicals and limited degree of conversion. Since the mobility is restricted severely from the early phases of the reaction, i.e. from the gel point, phase separation is suppressed despite any potential thermodynamic instability, and the copolymerization process is random. This was confirmed by identification of single glass transition temperature in DMA experiments of copolymers. Heterogeneous character of morphogenesis is related to a varying reactivity of pendant functional groups. In the early phases of the polymerization, propagation proceeds via intramolecular attack of the radical site to the pendant, leading to the primary cycle formation. Probability of the cyclization is increased by flexibility of the monomer backbone. Heterogeneity of the curing reaction is characterized by formation of internally crosslinked structures, i.e. microgels, followed by their interconnections. On contrary, rigidity of the monomer leads to a higher effectivity of crosslinking and more homogeneous morphology of the corresponding networks. Presence of the inhomogeneities, characterized by coexistence of structurally distinct regions, is related to a two-step mechanism of thermal decomposition. Progress of the storage modulus and the glass transition temperature correlate with the network stiffness, effectivity of crosslinking, and the presence of physical interactions that reinforce the structure beyond the scope of covalent crosslinking. Structural heterogeneity is manifested by broad transition region indicating wide variations in relaxation times. Experimental data are in qualitative correlation with the numerical models that simulates kinetics of free radical network polymerization.
Analýza vybraných lékových problémů u některých revmatických nemocí
Hromádková, Lucie ; Vlček, Jiří (vedoucí práce) ; Macek, Karel (oponent) ; Bradna, Petr (oponent)
Univerzita Karlova v Praze, Farmaceutická fakulta v Hradci Králové Katedra Katedra sociální a klinické farmacie Kandidát Mgr. Lucie Hromádková Školitel Prof. RNDr. Jiří Vlček, CSc. Název dizertační práce Analýza vybraných lékových problémů u některých revmatických nemocí. Úvod: Systémová onemocnění pojiva jsou specifická svým charakterem a často vyžadují dlouhodobou agresivní terapii více léky současně. Častá je však i nutnost léčby jiných, někdy souvisejících nemocí. Vyšší počet užívaných léků, přítomnost nepříjemných nežádoucích účinků a složitá dávkovací schémata mohou vytvářet vhodné prostředí pro vznik lékových problémů, jako jsou lékové interakce a léková compliance pacienta. Cíle: Cílem práce je analýza dvou lékových problémů, lékových interakcí a lékové compliance, v prostředí farmakoterapie systémových onemocnění pojiva. Cílem je vytvořit přehled interakcí glukokortikoidů, imunosupresiv a antimalarik s léky běžně se vyskytujícími v praxi, provést analýzu lékové compliance u pacientů se systémovou sklerodermií včetně zhodnocení možných rizikových faktorů non-compliance a shrnout dosavadní poznatky o lékové compliance u pacientů s revmatoidní artritidou. Metodika: Lékové interakce byly zpracovány systematickou rešerší literatury pomocí zdrojů: Micromedex, PubMed, Medline, Kompendium lékových...
Dlouhodobá odolnost okrajového uzávěru kompozitních výplní v prostředí se zvýšeným korozním rizikem
Roubíčková, Adéla ; Bradna, Pavel (vedoucí práce) ; Veverka, Jan (oponent) ; Halačková, Zdena (oponent)
Souhrn Úvod: Adhezní spoj mezi tvrdými zubními tkáněmi a kompozitními rekonstrukcemi je v ústní dutině vystaven působení mechanického zatížení, vody, bakterií, enzymů a chemických látek, které mohou jeho odolnost a tím i životnost celé rekonstrukce významně snižovat. Na rozdíl od rozsáhlého výzkumu degradačního vlivu vody, účinku chemických látek na adhezní spoj větší pozornost dosud věnována nebyla. Cíl: Cílem práce bylo objasnit vliv kosmetických peroxidových bělicích přípravků a prostředků ústní hygieny s chlorhexidinem a preventivních přípravků s fluoridy na odolnost adhezního spoje, vytvořeného několika různými adhezivními systémy metodou mikronetěsnosti (microleakage) na výplních V. třídy. Materiály a metodika: Použity byly "etch and rinse" adhezivní systém Gluma Comfort Bond (GLU) a "self-etch" adheziva Clearfil SE Bond (CLF), Adper Prompt (ADP) a iBond (IBO), reprezentující adhezivní systémy s různým pracovním postupem. Celkem bylo pro tyto experimenty použito 192 extrahovaných lidských molárů, které byly rekonstruovány mikrohybridním kompozitem Charisma a poté vystaveny působení peroxidového bělicího gelu Opalescence PF 20 s 20 % karbamid peroxidu, ústní vody Corsodyl s obsahem chlorhexidin diglukonátu a ústní vody Elmex s fluoridy. Expoziční časy byly 2 a 6 měsíců, peroxidový bělicí gel byl...
Vliv prostředí s korozním účinkem na dlouhodobou stabilitu adhezního spoje mezi sklovinou, dentinem a kompozitními materiály
Dudek, Michal ; Bradna, Pavel (vedoucí práce) ; Veverka, Jan (oponent) ; Halačková, Zdena (oponent)
Souhrn Úvod: Implementace adhezivních technologií do terapie zubního kazu přinesla rozpoznatelný pokrok do stomatologické praxe, projevující se nejen vysoce estetickým výsledkem ošetření, ale také možností ušetřit velký objem tvrdých zubních tkání, k jejichž ztrátám vedly dřívější výplňové technologie s invazivní preparací kazivých lézí pro dosažení mechanické retence výplňových materiálů. Včasné zastavení progrese zubního kazu pomocí adhezivních technologií vytvořilo předpoklady pro výraznější preventivní účinek ošetření zubního kazu, akcelerovaný neustále pokračujícím vývojem adhezivních prostředků a kompozitních materiálů, zajišťujících akceptovatelně dlouhou životnost z nich zhotovených rekonstrukcí. Adhezní spoje dentálních rekonstrukcí jsou v ústní dutině vystaveny různým mechanickým, chemickým a biologickým vlivům. Jedním z významných chemických agens jsou peroxidové bělicí gely, používané pro zesvětlení zubů. Tento kosmetický výkon je dnes ve stomatologické praxi velmi rozšířen. Účinnou látkou bělicích gelů je peroxid vodíku či jeho prekurzory, které při svém rozkladu uvolňují kyslíkové radikály, reagující s chromorforními molekulami pigmentů, usazených v tvrdých zubních tkáních. Volné radikály však reagují nespecificky, tj. nejenom s chromoforními molekulami, ale i s tvrdými zubními tkáněmi,...
Studium vlivu vlastností polymeračních lamp na vytvrzení kompozitních materiálů s různými fotoiniciačními systémy
Froněk, Jan ; Bradna, Pavel (vedoucí práce) ; Veverka, Jan (oponent)
Práce je zaměřena na sledování vlivu několika různých typů dentálních polymeračních lamp na vytvrzení kompozitních materiálů dimetakrylátového typu s kafrchinonovým a acylfosfinoxidovým iniciačním systémem a kompozitního materiálu epoxidového typu. Proměnnými parametry polymeračních lamp byly světelný výkon, charakter emisního spektra, tepelná emise a rozložení intenzity světla ve svazku světlovodu. Rozsah polymerace byl hodnocen měřením povrchové tvrdosti, parametry lamp radiometrickými metodami, teplotní změny polymerovaného materiálu termočlánkem. Výsledky byly zpracovány statisticky. Rozložení intenzity světla bylo hodnoceno metodou analýzy obrazu a ověřeno měřením rozložení tvrdosti v ozařované ploše polymerovaného materiálu. Cílem práce bylo získat nezávislé údaje o vlivu sledovaných parametrů na polymeraci kompozitních materiálů používaných v zubním lékařství, s dopadem na životnost kompozitních rekonstrukcí zubů a zátěž organismu látkami vyluhovanými z nedokonale polymerovaného materiálu.

Národní úložiště šedé literatury : Nalezeno 12 záznamů.   1 - 10další  přejít na záznam:
Viz též: podobná jména autorů
1 Bradna, Petr
Chcete být upozorněni, pokud se objeví nové záznamy odpovídající tomuto dotazu?
Přihlásit se k odběru RSS.