Název:
Microstructure of commercially pure titanium after cryogenic milling and spark Plasma sintering
Autoři:
Kozlík, J. ; Harcuba, P. ; Stráský, J. ; Chráska, Tomáš ; Janeček, M. Typ dokumentu: Příspěvky z konference Konference/Akce: 27th International Conference on Metallurgy and Materials, Brno (CZ), 20180523
Rok:
2018
Jazyk:
eng
Abstrakt: Commercially pure titanium was prepared by advanced powder metallurgy methods with the aim to produce the ultra-fine grained material. Cryogenic attritor milling was used as a first step to refine the microstructure at liquid argon temperatures to suppress recovery and dynamic recrystallization. Spark plasma sintering was subsequently employed to produce bulk material, exploiting its ability to achieve fully dense structure in short time and thus to reduce the grain growth. In order to understand the undergoing microstructural changes during the process, detailed investigation was performed after each preparation step. Powder morphology was changed significantly after milling, while particle fragmentation was only limited. Grain size after sintering was in micrometer scale, relatively independent of sintering conditions.
Klíčová slova:
Cryogenic milling; Microstructure; Spark plasma sintering; Titanium Zdrojový dokument: Metal 2018 - 27th International conference on metallurgy and materials, Conference Proceedings, ISBN 978-80-87294-84-0
Instituce: Ústav fyziky plazmatu AV ČR
(web)
Informace o dostupnosti dokumentu:
Dokument je dostupný v příslušném ústavu Akademie věd ČR. Původní záznam: http://hdl.handle.net/11104/0295555