Original title: Microstructure of commercially pure titanium after cryogenic milling and spark Plasma sintering
Authors: Kozlík, J. ; Harcuba, P. ; Stráský, J. ; Chráska, Tomáš ; Janeček, M.
Document type: Papers
Conference/Event: 27th International Conference on Metallurgy and Materials, Brno (CZ), 20180523
Year: 2018
Language: eng
Abstract: Commercially pure titanium was prepared by advanced powder metallurgy methods with the aim to produce the ultra-fine grained material. Cryogenic attritor milling was used as a first step to refine the microstructure at liquid argon temperatures to suppress recovery and dynamic recrystallization. Spark plasma sintering was subsequently employed to produce bulk material, exploiting its ability to achieve fully dense structure in short time and thus to reduce the grain growth. In order to understand the undergoing microstructural changes during the process, detailed investigation was performed after each preparation step. Powder morphology was changed significantly after milling, while particle fragmentation was only limited. Grain size after sintering was in micrometer scale, relatively independent of sintering conditions.
Keywords: Cryogenic milling; Microstructure; Spark plasma sintering; Titanium
Host item entry: Metal 2018 - 27th International conference on metallurgy and materials, Conference Proceedings, ISBN 978-80-87294-84-0

Institution: Institute of Plasma Physics AS ČR (web)
Document availability information: Fulltext is available at the institute of the Academy of Sciences.
Original record: http://hdl.handle.net/11104/0295555

Permalink: http://www.nusl.cz/ntk/nusl-394144


The record appears in these collections:
Research > Institutes ASCR > Institute of Plasma Physics
Conference materials > Papers
 Record created 2019-04-15, last modified 2022-09-29


No fulltext
  • Export as DC, NUŠL, RIS