Biodegradable bones implants based on Fe
Tkáčová, Tereza ; Míka, Martin (referee) ; Sedlaříková, Marie (advisor)
This thesis writes about biodegradable bone implants based on iron. The currently used metal-based implants have disadvantage in an often need of secondary surgery intervention to remove the implant. Therefore, there is a big research of biodegradable bone implants nowadays. In this work, iron-based materials with the addition of zinc and magnesium are being investigated. The produced samples have been immersed in a solution of NaCl and simulated body fluid, SBL. Subsequently there were regularly analysed changes of corrosion potential, pH, conductivity and also weight loss was watched.
Biodegradable bones implants based on Fe
Tkáčová, Tereza ; Míka, Martin (referee) ; Sedlaříková, Marie (advisor)
This thesis writes about biodegradable bone implants based on iron. The currently used metal-based implants have disadvantage in an often need of secondary surgery intervention to remove the implant. Therefore, there is a big research of biodegradable bone implants nowadays. In this work, iron-based materials with the addition of zinc and magnesium are being investigated. The produced samples have been immersed in a solution of NaCl and simulated body fluid, SBL. Subsequently there were regularly analysed changes of corrosion potential, pH, conductivity and also weight loss was watched.
Adhesion, growth and differentiation of osteoblast-like cells on materials for bone implants
Doubková, Martina ; Bačáková, Lucie (advisor) ; Filová, Eva (referee)
This thesis focuses on testing and improving Ti-6Al-4V ELI biomaterials, which are currently one of the most used titanium alloys in biomedicine (predominantly in orthopaedics and dentistry), in cooperation with research institutions and private companies developing and producing such materials. The metallic samples were previously modified by plasma electrolytic oxidation (PEO) with use of electrolytes of a different composition to induce development of a homogeneous TiO2 layer on its surface. In vitro interactions of human osteoblast-like cell line Saos-2 with the surface of Ti-6Al-4V ELI alloy samples are investigated. Initial cell attachment, spreading, morphology, cell population density, viability, calcium deposition and expression of selected osteogenic markers, e.g. collagen type I, alkaline phosphatase and osteocalcin, were evaluated on cultured cells. The cells behavior were then correlated with physicochemical properties of the material surface, such as its topography, roughness, wettability, surface layer chemical composition etc. The results are also compared with those obtained in cells cultured on control samples of untreated alloys as well as microscopic glass coverslips and bottom of standard polystyrene cell culture wells. The aim of this thesis is to select the most promising...
Growth of human adipose-derived stem cells on Ti-6Al-4V alloy with various surface modifications
Kročilová, Nikola ; Bačáková, Lucie ; Pařízek, Martin ; Havlíková, Jana ; Motarjemi, H. ; Molitor, M. ; Gabor, R. ; Marvan, J.
Adipose-derived stem cells (ASCs) are of a great importance for bone tissue engineering. We compared ASCs obtained by liposuction under two pressures (-200 mmHg and -700 mmHg). The number and proliferation activity of cells isolated under -700 mmHg (ASC-H) were higher than in cells isolated under -200 mmHg (ASC-L). However, the ASC-L was more active in osteogenic differentiation, as manifested by a higher intensity of fluorescence of alkaline phosphatase and osteocalcin in these cells. The adhesion and growth of ASCs were then studied on Ti-6Al-4V samples either unmodified (K, roughness parameter R-a = 280 nm) or modified by shot blasting and tarnishing A, R-a = 200 nm), vibratory finishing (B, R-a = 100 nm) and vibratory finishing, shot blasting and polishing (C, R-a = 80 nm). All modified samples were more wettable than the K samples. On day 1 after seeding, the size of cell spreading area on some modified samples was lower than on K samples, namely on B samples in ASC-L, on B and C in ASC-H and on A in control MG-63 cells. On day 3, the cell number on some modified samples became higher than on K samples, namely on C samples (ASC-L), on B (ASC-H) and on B and C s (MG-63 cells). On day 7, the numbers of ASC-H and MG-63 cells on all modified samples evened out and became significantly higher than on K samples. On ASC-L samples, the highest cell numbers were obtained on A samples. Thus, all studied modifications of Ti-6Al-4V enhanced growth of ASCs and human osteoblast-like MG-63 cells.
Growth and differentiation of human osteoblast-like cells on TI-6AL-4V alloy modified with anodization
Doubková, Martina ; Bačáková, Lucie ; Pařízek, Martin ; Vandrovcová, Marta ; Musílková, Jana ; Lisá, Věra ; Gabor, R. ; Marvan, J.
Titanium and its alloys are widely used as hard tissue implants for their high biocompatibility and suitable physical properties. Along with other surface treatment methods, anodization technique is known to enhance osseointegration. The aim of this study is to evaluate the adhesion, growth and osteogenic differentiation of human osteoblast-like SAOS-2 cells on Ti-6Al-4V samples anodized in electrolytes composed of a stable volume of KOH (336.48 g/l) and variable volumes of liquid glass (124.47 g/l, 84,12 g/l and 37.38 g/l; samples s5, s6 and s7, respectively). Non-anodized Ti-6Al-4V samples, cell culture polystyrene (PS) and microscopic glass coverslips served as control materials. On days 2 and 4 after seeding, the cell number did not differ significantly among the tested samples. However, on day 7, the cell number on s6 samples reached the lowest values, which could be attributed to a non-homogeneous TiO2 film on s6 samples formed during anodization. Nevertheless, the osteogenic differentiation, estimated by the intensity of fluorescence of collagen I in cells grown in a differentiation medium, was the highest on s6 samples. On s5 samples, coated with homogeneous TiO2 films, both cell numbers and intensity of fluorescence of collagen I was relatively high. The bone matrix mineralization, evaluated by Alizarin Red staining, was the highest on s5 samples in standard culture medium, and similar on all tested samples in differentiation medium. Thus, the surface modification of s5 samples could be considered the most suitable for application in bone implants.
Polymeric nanofibrous scaffolds reinforced with diamond and ceramic nanoparticles for bone tissue engineering
Bačáková, Lucie ; Pařízek, Martin ; Staňková, Ľubica ; Novotná, Katarína ; Douglas, T.E.L. ; Brady, M. A. ; Kromka, Alexander ; Potocký, Štěpán ; Stránská, D.
Three types of nanofibrous scaffolds were prepared by electrospining: (1) poly(lactide-co-glycoside) (PLGA) scaffolds reinforced with 23 wt.% of diamond nanoparticles (DNPs), (2) poly(L-lactide) (PLLA) scaffolds with DNPs in concentration ranging from from 0.4 wt.% to 12.3 wt.%, and (3) PLLA scaffolds with 5 wt.% or 15 wt.% of hydroxyapatite (HAp) nanoparticles. The diameter of the nanofibers ranged between 160 and 729 nm. The nanofibers with nanoparticles were thicker and the void spaces among them were smaller. Mechanical properties of the nanoparticle-loaded scaffolds were better, as demonstrated by a rupture test in scaffolds with DNPs and by a creep behavior test in scaffolds with HAp. On PLGA scaffolds with DNPs, the human osteoblast-like MG-63 cells adhered in similar numbers and grew with similar kinetics as on pure PLGA scaffolds. Human bone marrow mesenchymal stem cells grew faster and reached higher population densities on PLGA-DNP scaffolds. However, on PLLA-based scaffolds, the activity of mitochondrial enzymes and concentration of osteocalcin in MG-63 cells decreased with increasing DNP concentration. On the other hand, the metabolic activity of MG-63 cells and content of osteocalcin in these cells were positively correlated with the HAp concentration in PLLA scaffolds. Thus, PLGA nanofibers with 23 wt% of DNPs and PLLA nanofibers with 5 and particularly 15 wt.% of HAp seem to be promising for bone tissue engineering.