Boronized stainless steel with zirconia coatings
Brožek, Vlastimil ; Kolísko, J. ; Kubatík, Tomáš František ; Mastný, L. ; Pokorný, P. ; Tej, P.
Conditions of boronizing are described using a reactive diffusion method of boron from boron carbide and lanthanum hexaboride so that the formation of Fe2B is preferred to FeB which is more brittle and whose structure does not satisfy the conditions for perfect adhesion of modified zirconia ceramics. Perfectly rigid adhesive connection of needle-like embedded interlayers Fe2B in steel AISI 303 prepared by reactive diffusion of a boronizing medium without activators at 1000 ° C and exposure of 2-4 hours has the value of 20 - 24 MPa at the Pinn-off test.Ceramic coatings from Al2O3-ZrO2 ceramics formed on those interlayers have the value of bond strength up to 14 - 20 MPa.Thermal cycling between 100°C - 600 °C confirmed good adhesion of coatings with the underlying steel.During thermal cycling at elevated temperatures (600-1000 °C) there occurs a statistically significant number of faults in cohesion and mechanical destruction of the coatings. One of the reasons are secondary changes

Interested in being notified about new results for this query?
Subscribe to the RSS feed.