Mesoporous TiO2 films with variable thickness were prepared by dip-coating. Two kinds of sols were used, sol 1 and sol 2, which were separately tested and compared. The activity of samples of these sols was tested employing photocatalytic degradation of 1.10-4 mol.dm-3 4-chlorphenol. The efficiency of the degradation of 4-chlorphenol was increasing proportionately with each additional layer. The optimum turned out to be three layers.
Analysis of trace pollutants in water and their photocatalytic degradation
Štěpánková, Sandra ; Rathouský, Jiří (advisor) ; Nesměrák, Karel (referee)
Mesoporous TiO2 films with variable thickness were prepared by dip-coating. Two kinds of sols were used, sol 1 and sol 2, which were separately tested and compared. The activity of samples of these sols was tested employing photocatalytic degradation of 1.10-4 mol.dm-3 4-chlorphenol. The efficiency of the degradation of 4-chlorphenol was increasing proportionately with each additional layer. The optimum turned out to be three layers.

Interested in being notified about new results for this query?
Subscribe to the RSS feed.