Long-term tests for examination of surface treatments in various adverse environments simulating real effects
Hudečková, Petra ; Vacula, Miroslav (referee) ; Bydžovský, Jiří (advisor)
Cement bonded particleboards contain organic base and as they are set outside, extreme weather condition, such as frost, chemical defrosting substances or sulphates, cause their degradation. The presence of the organic base in the matrix of the material could be the reason why there is higher probability of degrading when compared with materials containing an inorganic base. It could be partially eliminated by an appropriate surface modification of the slab, which main goal is to weaken the impact of an aggressive environment and to extend the lifespan of the board. On the other hand, the surface modifications based on a polymer base are prone to degrade because of other unfavourable conditions such as UV radiation when compared with the cement bonded particleboard. The classification of the surface modifications and the way of their degradation caused by the aggressive environment in real applications are presented in the theoretical part of the thesis. In the experimental part, appropriate methodical ways of testing the resistance of cement bonded particleboard’s coating system were chosen. Then, the testing and comparing of the physical, mechanical and aesthetic properties of different types of coatings were done. Moreover, a spectrophotometric analysis of the colour shade changes for the different aggressive environment were carried out. Furthermore, microstructures of chosen surface modifications were assessed by using an optical and an electron microscope.
|
|
Surface hardening of cast iron by high power diode laser
Bezděk, Pavel ; Daněk, Ladislav (referee) ; Mrňa, Libor (advisor)
The Master’s thesis deals with the technology of surface hardening by laser. High power diode laser is used for this purpose. Surface hardening is performed on cast iron BS 1452-77, at different speeds laser head and laser power. In introduction, the theoretical part deals with possible ways of hardening focusing on the benefits of laser hardening. There are mentioned basic parts of laser, type industrial lasers and their application in industry. The final part is mentions the using of material and methods used to evaluate samples. The practical part describes the using devices and carries out evaluation macrostructure and microstructure and evaluation of hardness depending on the distance from the surface.
|
|
Study of the effect of selected types of aditives on the properties of cement composites
Kavka, Lukáš ; Ťažký, Tomáš (referee) ; Bodnárová, Lenka (advisor)
The diploma thesis describes admixtures for concrete. It deals with the influence of admixtures on the properties of cement composites in the fresh and hardened state. The theoretical part described the individual components of concrete, where the main attention was focused to inert admixtures and their effect on mechanical properties, shrinkage, resistance of cement composites to aggressive medium. Furthermore, the effect of admixtures on concretes with recycled aggregates was described. In the first stage of the practical part, cement mortars with 25, 35 and 50% replacement of cement admixtures were created. In the second stage, concretes with admixtures and a minimum strength class of C30/37 and C50/60 were created. Finely ground granulated slag, micronized limestone and granite stone dust were used as admixtures in mortars and concretes. The change of properties in the fresh and hardened state was observed on cement composites.
|
|
Study of the effect of selected types of aditives on the properties of cement composites
Kavka, Lukáš ; Ťažký, Tomáš (referee) ; Bodnárová, Lenka (advisor)
The diploma thesis describes admixtures for concrete. It deals with the influence of admixtures on the properties of cement composites in the fresh and hardened state. The theoretical part described the individual components of concrete, where the main attention was focused to inert admixtures and their effect on mechanical properties, shrinkage, resistance of cement composites to aggressive medium. Furthermore, the effect of admixtures on concretes with recycled aggregates was described. In the first stage of the practical part, cement mortars with 25, 35 and 50% replacement of cement admixtures were created. In the second stage, concretes with admixtures and a minimum strength class of C30/37 and C50/60 were created. Finely ground granulated slag, micronized limestone and granite stone dust were used as admixtures in mortars and concretes. The change of properties in the fresh and hardened state was observed on cement composites.
|
|
Long-term tests for examination of surface treatments in various adverse environments simulating real effects
Hudečková, Petra ; Vacula, Miroslav (referee) ; Bydžovský, Jiří (advisor)
Cement bonded particleboards contain organic base and as they are set outside, extreme weather condition, such as frost, chemical defrosting substances or sulphates, cause their degradation. The presence of the organic base in the matrix of the material could be the reason why there is higher probability of degrading when compared with materials containing an inorganic base. It could be partially eliminated by an appropriate surface modification of the slab, which main goal is to weaken the impact of an aggressive environment and to extend the lifespan of the board. On the other hand, the surface modifications based on a polymer base are prone to degrade because of other unfavourable conditions such as UV radiation when compared with the cement bonded particleboard. The classification of the surface modifications and the way of their degradation caused by the aggressive environment in real applications are presented in the theoretical part of the thesis. In the experimental part, appropriate methodical ways of testing the resistance of cement bonded particleboard’s coating system were chosen. Then, the testing and comparing of the physical, mechanical and aesthetic properties of different types of coatings were done. Moreover, a spectrophotometric analysis of the colour shade changes for the different aggressive environment were carried out. Furthermore, microstructures of chosen surface modifications were assessed by using an optical and an electron microscope.
|
|
Surface hardening of cast iron by high power diode laser
Bezděk, Pavel ; Daněk, Ladislav (referee) ; Mrňa, Libor (advisor)
The Master’s thesis deals with the technology of surface hardening by laser. High power diode laser is used for this purpose. Surface hardening is performed on cast iron BS 1452-77, at different speeds laser head and laser power. In introduction, the theoretical part deals with possible ways of hardening focusing on the benefits of laser hardening. There are mentioned basic parts of laser, type industrial lasers and their application in industry. The final part is mentions the using of material and methods used to evaluate samples. The practical part describes the using devices and carries out evaluation macrostructure and microstructure and evaluation of hardness depending on the distance from the surface.
|