Quantum-mechanical study of magnetic properties of superalloy nanocomposite phase Fe2AlTi
Slávik, Anton ; Miháliková, Ivana ; Friák, Martin ; Všianská, Monika ; Šob, Mojmír
The L21-structure Fe2AlTi intermetallic compound is one of the two phases identified in Fe-Al-Ti superalloy nanocomposites. Experimental data related to low-temperature magnetic properties of this Heusler compound indicate that magnetic moment is about 0.1 Bohr magneton per formula unit. In contrast, previous quantum-mechanical calculations predicted Fe2AlTi to have much higher magnetic moment, 0.9 Bohr magneton per formula unit. In order to solve this discrepancy between the theory and experiment we have performed a series of quantum-mechanical fix-spin-moment calculations and compared our results with those for non-magnetic state. It turns out that the total energy of the non-magnetic state is only by 10.73 meV/atom higher than that of the magnetic state. When applying Boltzmann statistics to this very small energy difference we predict that the non-magnetic state appears at non-zero temperatures with significant probabilities (for instance, 22.36 % at T = 100 K) and reduces the overall magnetic moment. As another mechanism lowering the magnetization we studied selected shape deformations, in particular trigonal shearing. Fe2AlTi exhibits a compression-tension asymmetry with respect to these strains and, for example, the strain 0.08 destabilizes the spin-polarized state, leaving the non-magnetic state as the only stable one.
First-principles study of interface energies in Fe-Al-based superalloy nanocomposites
Miháliková, Ivana ; Slávik, Anton ; Friák, Martin ; Všianská, Monika ; Koutná, N. ; Holec, David ; Šob, Mojmír
Fe-Al-based nanocomposites with a superalloy-type of microstructure constitute a very promising class of materials. They possess a great potential as an alternative to the currently used steel grades in high temperature applications. Intermetallics-containing nanocomposites, such as those with the Fe3Al compound being one of the phases, may open a way towards future automotive and energy-conversion technologies with lower fuel consumption and reduced environmental impact. We employ quantum-mechanical calculations to analyze relations between ordering tendencies of Al atoms in the disordered Fe-18.75at.%Al phase on one hand and thermodynamic, structural and magnetic properties of Fe-Al-based nanocomposites on the other. When comparing supercells modeling disordered Fe-Al phase with different atomic distribution of atoms we find out that the supercell without 1st and 2nd nearest neighbor Al-Al pairs has a lower energy than that mimicking a perfect disorder (a special quasi-random structure, SQS). Further, coherent interfaces with (001), (110) and (1-10) crystallographic orientations between Fe3Al compound and SQS Fe-Al phase have higher energies than those exhibiting atomic distribution without 1st and 2nd nearest neighbor Al-Al pairs.